Some basic information about the DSC (Differential Scanning Calorimetry) test
The DSC (Differential Scanning Calorimetry) test is an analytical technique used to examine and characterize the thermal behaviour of materials. This test is used to measure the reaction of a material to changes in temperature and its thermal properties.
DSC is widely used in material science, chemistry, pharmaceutics, food science and many other fields.
The DSC test operates by comparing two different samples (usually one reference sample and one test sample). Basically, the samples are subjected to the same temperature program and then the heat exchange is observed. The DSC curves show the heat flow changes in response to temperature. These changes are a reflection of thermal phenomena such as phase transition, melting or crystallization.
RELATED SUBJECTS
- ASTM D6653 High Altitude Package Test: Simulating Vacuum Conditions for Packaging Integrity
- Crack Propagation Test in Plastics: Why It Matters and How to Apply It
- ISO 178 - 3-Point Test Device
- Methods for Measuring Material Durability Using ISO 37 Tensile Testing
- Shoe Testing Devices and Their Functions: Measuring Quality and Durability
- What Are Quality Control Test Equipment?
- What Is A Compression Test?
- What Is A Shore Hardness Test?
- What Is An MFI (Melt Flow Index) Test?
- What is a Ring Stiffness Test Device and How is it Used?