Some basic information about the DSC (Differential Scanning Calorimetry) test
The DSC (Differential Scanning Calorimetry) test is an analytical technique used to examine and characterize the thermal behaviour of materials. This test is used to measure the reaction of a material to changes in temperature and its thermal properties.
DSC is widely used in material science, chemistry, pharmaceutics, food science and many other fields.
The DSC test operates by comparing two different samples (usually one reference sample and one test sample). Basically, the samples are subjected to the same temperature program and then the heat exchange is observed. The DSC curves show the heat flow changes in response to temperature. These changes are a reflection of thermal phenomena such as phase transition, melting or crystallization.
RELATED SUBJECTS
- Peel Test on Tedlar PVF Films: Methods for Measuring Coating and Adhesive Durability
- UL 94 Flammability Tests
- What Is A Compression Test?
- What Is ECT (Edge Crush Test)?
- What Is Halogen-Free and Why Is It Important?
- What Is RCT (Ring Crush Test)?
- What Is a Film Adhesion and Durability Test Device?
- What Is an Air Spring Test Device?
- What is the Rubber Glove Tensile Test?
- What is the Schopper Test and How is it Performed?