Some basic information about the DSC (Differential Scanning Calorimetry) test
The DSC (Differential Scanning Calorimetry) test is an analytical technique used to examine and characterize the thermal behaviour of materials. This test is used to measure the reaction of a material to changes in temperature and its thermal properties.
DSC is widely used in material science, chemistry, pharmaceutics, food science and many other fields.
The DSC test operates by comparing two different samples (usually one reference sample and one test sample). Basically, the samples are subjected to the same temperature program and then the heat exchange is observed. The DSC curves show the heat flow changes in response to temperature. These changes are a reflection of thermal phenomena such as phase transition, melting or crystallization.
RELATED SUBJECTS
- Air Springs Tests - Air Suspension Bellows
- Crack Propagation Test in Plastics: Why It Matters and How to Apply It
- Glass Material Bending Test Device
- ISO 178 - 3-Point Test Device
- What Is Four-Point Bending Test?
- What Is a Thermal Cycling Test Chamber and How Does It Work?
- What is Elmendorf Tear Strength?
- What is a Torque Wrench and Where is it Used?
- What is the Charpy-Izod (Notched) Impact Test and How is it Performed?
- What is the ISTA Packaging Test? Packaging Durability Test According to International Standards